The use of pegmatite of the Chupinskoye deposit with admixtures of mica for the production of porcelain glaze may cause the formation of a "prickly" glaze defect. It was found that the introduction of calcined kaolin into the composition of the cobalt feldspar glaze reduces the likelihood of this defect formation. Tab. 1, bibliography: 4 titles.
Platov Yu. T., Platova RA, Sorokin DA Assessment of porcelain whiteness // Glass and ceramics. 2008. N 8.P. 23 - 27. Platov Yu. T., Platova RA, Sorokin DA Evaluation of porcelain whiteness // Glass and Ceram. 2008. V. 65. N7-8. R. 272 ??- 277. Pyzhova A.P., Korobkina V.V., Kosov V.S. Defects of toned-ceramic products. Moscow: Legprombytizdat, 1993.176 p. Maslennikova G. N., Andreeva T. F. Basic properties of glazes for high-voltage porcelain. Survey information. M .: Informelektro, 1976.52 p. Maslennikova G. N., Kharitonov F. Ya. Fundamentals of calculating the compositions of masses and glazes in electroceramics. Moscow: Energiya, 1978.144 p.

The article can be purchased
electronic!

PDF format

Not on sale

UDK 666.295
Article type: Science for ceramic production
Make a request

Keywords

Use the reference below to cite the publication

T. L. Neklyudova and S. A. Akent'ev Reduction of the probability of pinhole formation in cobalt feldspathic glazes used in porcelain production. Steklo i keramika. 2011:84(3):16-17. (in Russ). UDK 666.295